Petroferm’s Lenium GS precision solvent has been approved by Boeing per its BAC 5408 Vapor Degreasing Specification (PSD 6-68).

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Petroferm’s Lenium GS precision solvent has been approved by Boeing per its BAC 5408 Vapor Degreasing Specification (PSD 6-68). The solvent is based on stabilized n-propyl bromide and is designed to operate in open-top and vacuum vapor degreasing equipment. It has been used as a drop-in replacement for trichloroethylene, HCFC-141b, HCFC-225, hydrofluoroethers, hydrofluorocarbons, perchloroethylene and methylene chloride.

The solvent also is approved for cleaning components by Bell Helicopter, Praxair and Scott Aviation. 