Designed for plating on metal substrates, Enthone’s Elpelyt GS-7 bright nickel process reduces the number of buffing and polishing steps, and decreases nickel metal consumption.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Designed for plating on metal substrates, Enthone’s Elpelyt GS-7 bright nickel process reduces the number of buffing and polishing steps, and decreases nickel metal consumption. Increased leveling power over traditional bright nickel processes helps decrease costs and increase performance, the company says. 