Company will introduce the new Standart® PCS Aluminum Powder at the.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Company will introduce the new Standart® PCS Aluminum Powder at the. PCS is the newest generation of high performance aluminum pigments, which are completely encapsulated with a stabilized surface coating that provides excellent chemical resistance. PCS is available in five different particle size grades that enable a range of optical effects.