EPi’s Kool-Blak mid-temperature blackening system is designed to deliver a durable, black oxide finish without smut. The finish, which meets military specs MIL-DTS 13924D and AMS 2458H, offers abrasion resistance without chipping, peeling or rubbing off. It blackens at 220-245°F and does not produce caustic boiling fumes, resulting in energy cost savings and a safer work environment for machine operators, the company says.