The SMT850 Plus from Klingspor combines non-woven and coated abrasives in one flap disc.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

 

The SMT850 Plus from Klingspor combines non-woven and coated abrasives in one flap disc. The disc is designed to offer a high rate of stock removal and a quality surface finish. According to the company, this leads to fewer processing steps and reduces machining times. The 4.5-inch discs are available in three different finishing grades: coarse, medium and very fine.

 