Gema's OptiFlex2 F Spray Unit Uses Advanced Pump Technology

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

This spray unit is based on Smart Inline Technologies.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon
�

Gema, OptiFlex2

Gema’s OptiFlex2 F Spray manual unit is designed for applications that require high-film builds or precise and constant powder outputs, when using long powder hoses. The unit is engineered for coating consistency and quality. The unit’s single-chamber design based on the Smart Inline Technologies enables a constant and reproducible coating result over a long period of time, even with challenging powders. Gema says the unit is engineered for easy and quick color changes and powder savings of up to 15 percent. 