Cleanguard High Strength addresses industry requirements for a heavy-duty protective floor covering.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon
Cleanguard High Strength addresses industry requirements for a heavy-duty protective floor covering. Its makers say this solvent and waterproof product is exceptionally durable providing prolonged service life to reduce change-outs for improved profitability. The white, textured and 100% lint free floorcovering traps and holds dust & dirt for a cleaner/brighter work area and fewer finishing rejects. Available in 600 foot-long rolls in widths of 36, 42 and 60 inches.