This process controls humidity in powder coating environmental rooms, saving energy costs up to 50% while improving quality.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

This process controls humidity in powder coating environmental rooms, saving energy costs up to 50% while improving quality. The company’s exclusive control system (patent pending) effectively controls both temperature and humidity in the environmental room.  It can be retrofitted to existing rooms or included with new turnkey modular units. “Anybody can control temperature,” said CEO Michael Napadow.  “Controlling humidity is difficult.  Our system can control moisture to within one percent of desired setting. It is the only system that can do that.”

 