The Model RX-400 rotary indexing finishing system present on or more fixtured components to the blast from multi-adjustable nozzles at a single blast station.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

The Model RX-400 rotary indexing finishing system present on or more fixtured components to the blast from multi-adjustable nozzles at a single blast station. Oscillating motion of the blast guns is said to enable rapid and complete coverage of target surfaces with a minimum number of nozzles and lower compressed air requirements. The system has protective features for use with harsh grit abrasives in production blast treatment operations such as etching, descaling and surface preparation.