Intech Services announces the newest addition to the Teflon coating line: 857G-3310.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Intech Services announces the newest addition to the Teflon coating line: 857G-3310. The water-based, green primer is acid free and is an alternative solution for those with VOC reduction initiatives. According to the company, 857G-3310 offers all the high-quality Teflon performance without the harshness of an acid-based primer. The new water-based primer is in stock and ready to ship. Sold by the gallon, 857G-3310 is compatible with high-build PTFE topcoats.