Jotun has added two two-component, solvent-based inorganic zinc ethyl silicate primers to its Resist coatings line.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Jotun has added two two-component, solvent-based inorganic zinc ethyl silicate primers to its Resist coatings line.

Resist 65 is designed to protect steel substrates exposed to corrosive environments and can be used as the first coat in a multiple-layer system for long-term protection. Resist ZES is best-suited for blast-cleaned steel and can be used in combination with advanced coating systems to further improve protection against corrosion.

Jotun Paints, call 800-229-3538 or visit jotun.com