Lanthane Blue 126 is Coventya Inc.'s latest addition to its Lanthane line of trivalent passivate technologies.A high-performance, single-component, low-temperature process, the passivate provides high performance (greater than 120 hours to WR) and a pronounced blue cast.

Related Topics:

Related Suppliers

Lanthane Blue 126 is Coventya Inc.'s latest addition to its Lanthane line of trivalent passivate technologies.

A high-performance, single-component, low-temperature process, the passivate provides high performance (greater than 120 hours to WR) and a pronounced blue cast. According to the company, Lanthane Blue 126 can be applied to all zinc electrolytes and is suitable for rack and barrel applications.