Pavco Inc. offers a line of zinc-nickel alloy technology for metal finishing.

Related Suppliers

Pavco Inc. offers a line of zinc-nickel alloy technology for metal finishing. For alkaline processes, the company’s Ziniloy 3028 can meet demanding requirements, while Ziniloy HD adds effective ductility characteristics. For chloride, NiClipse C provides uniform alloy deposit through a range of current densities for productivity and direct plating on cast iron substrates.

The company’s metal finishing technologies are intended to meet the ever-increasing demands of the industry for decorative hex chrome alternatives and general metal-finishing-compliant chemistries. 

Editor Pick

NY/NJ's Masters Association of Metal Finishers Honors Members

Honorees included Walter Schwartz, who received the Award of Special Recognition for his work in the industry, and New Brunswick Plating, which received the Stephen Candiloro Memorial Award.

Related Topics