Crack Formation during Electrodeposition and Post-deposition Aging of Thin Film Coatings - 5th Quarterly Report

This NASF-AESF Foundation research project report covers the fifth quarter of project work (January-March) on this AESF Foundation Research project at the University of Houston. The objective of the work is to study fundamental and practical aspects of crack formation in electrodeposited thin films.
#nasf #basics #plating

Electroplating

AES Research Project 3, Adhesion of Electrodeposits, Prologue

This is the prologue for a four-part article consisting of the full report of AES Research Project #3, Adhesion of Electrodeposits, done at the University of Michigan in the mid-1940s, following the end of World War II.
#basics #plating

Electroplating

AES Research Project 3, Adhesion of Electrodeposits, Part 1, Bibliography

This is Part 1 of a four-part article consisting of the full report of AES Research Project #3, Adhesion of Electrodeposits, done at the University of Michigan in the mid-1940s, following the end of World War II. It consists of the complete bibliography compiled during the project.
#basics #plating

Electroplating

AES Research Project 3, Adhesion of Electrodeposits, Part 2, General Considerations

This is Part 2 of a four-part article consisting of the full report of AES Research Project #3, Adhesion of Electrodeposits, done at the University of Michigan in the mid-1940s, following the end of World War II. It outlines the general concepts involved on plate adhesion.
#basics #plating

Electroplating

AES Research Project 3, Adhesion of Electrodeposits, Part 3, Publications Review on Measurement

This is Part 3 of a four-part article consisting of the full report of AES Research Project #3, Adhesion of Electrodeposits, done at the University of Michigan in the mid-1940s, following the end of World War II. It reviews the published methods for measuring adhesion.
#basics #plating

Electroplating

AES Research Project 3, Adhesion of Electrodeposits, Part 4, Commentary on Measurement

This is Part 4 of a four-part article consisting of the full report of AES Research Project #3, Adhesion of Electrodeposits, done at the University of Michigan in the mid-1940s, following the end of World War II. It contains a commentary by industry people on the published methods for measuring adhesion.
#basics #plating

Electrocoating

Author: Time for EPA to Lead in 'Real World' Safety Standards

"I implore our new administration in Washington to take the lead and bring good sense and reason back into the regulatory process."
#plating #pollutioncontrol #basics

Electroplating

The Systems View in Automotive Finishes: Essential, but Overlooked - The 38th William Blum Lecture

This article is a re-publication of the 38th William Blum Lecture, presented at the 84th AES Annual Convention in Detroit, Michigan on June 23, 1997.  This lecture reviews a number of works in automotive finishing R&D in which understanding of the overall system was absolutely essential to success, from classical nickel-chromium plating to work in vacuum/electroplated hybrids for plated plastics, electrogalvanized zinc and hard chromium in stamping dies.
#automotive #basics #plating

Electroplating

Faraday's Children (and Nickel): The 40th William Blum Lecture

This article is a republication of the 40th William Blum Lecture, presented at the 86th AESF Annual Convention in Detroit, Michigan on June 21, 1999. In this lecture, Dr. George DiBari describes the search for the ideal nickel anode material and the outlook for survival of nickel plating at the end of the 20th century.
#surfin #basics #plating

Electroplating

Automated Electroplating Systems

Simultaneous engineering reduces energy and resource consumption.
#basics #plating #energy