ELECTROPLATING WHITEPAPERS

Electroplating

Experimental Study on the Formation of Electroless Nickel-Boron Coatings from a Borohydride-Reduced Bath on Mild Steel

This paper is a peer-reviewed and edited version of a presentation delivered at NASF SUR/FIN 2012 in Las Vegas, Nev., on June 13, 2012.
#research #nasf #surfin

Electroplating

Hexavalent Chromium - What Else?

Dr. Patrick Benaben won the 2011 NASF Scientific Achievement Award. Here is an edited version of his presentation at NASF SUR/FIN 2012, along with commentary provided by Dr. James H. Lindsay, Technical Editor for the NASF.
#research #nasf #surfin

Electroplating

Method for Comparison of Leveling in Decorative Acid Copper Plating

Presented here is a test mechanism used to compare and contrast systems for leveling in acid copper plating as well as additives within a system.
#research

Electroplating

White Bronze, Copper-Tin-Zinc Tri-metal: Expanding Applications and New Developments in a Changing Landscape

This paper deals with the renewed interest in applications for white bronze tri-metal (Cu-Sn-Zn alloy).
#research

Electroplating

Corrosion Resistance of High-Phosphorus Electroless Nickel with a Lower Coefficient of Friction, Nanoparticle Codeposition Electroless Nickel Layer

This paper is a peer-reviewed and edited version of a presentation delivered at NASF SUR/FIN 2013 in Rosemont, Ill., on June 11, 2013.
#research #nasf #surfin

Electroplating

Electrodeposition of Ni-Fe-Mo-W Alloys - Part 1

This paper was submitted to NASF and the AESF Foundation Research Board in April 2013 as a 1st-quarter report of AESF Research Project #R-117.
#research #nasf

Electroplating

Electrodeposition of Ni-Fe-Mo-W Alloys - Part 2

This paper was submitted to NASF and the AESF Foundation Research Board in July 2013 as a 2nd-quarter report of AESF Research Project #R-117.
#nasf #research

Electroplating

Electroplated Tin-Nickel Coatings as a Replacement for Nickel to Eliminate Nickel Dermatitis

This paper is a peer-reviewed and edited version of a paper delivered at NASF SUR/FIN 2013 in Rosemont, Ill., on June 12, 2013.
#research #surfin #nasf

Electroplating

Alloy Plating by Heating Stacked Single Layers and the Possibility of its Application in the Future

This paper was presented at NASF SUR/FIN 2013 in Rosemont, Ill., on June 10, 2013.
#surfin #research #nasf

Electroplating

Selective Brush Plating a Tin-Zinc Alloy for Sacrificial Corrosion Protection

A tin-zinc selective brush plated coating has been developed to provide sacrificial corrosion protection without the use of toxic chemicals.
#research #surfin