You are viewing products related to: Electroless Plating (Ni, Cu, Au)

PUBLISHED: 6/30/2017

Chrome-Free Aerospace Sealant Features Lightweight, Corrosion-Inhibiting Properties

PPG offers a chrome-free aerospace sealant designed for aircraft manufacturers and maintenance, repair and overhaul shops requiring corrosion-inhibiting properties.


PUBLISHED: 5/2/2017

Techmetals Specializes in Anodizing, Coatings, Metal Finishing Applications

Processes include electroless nickel, nickel Teflon, nickel boron, composite diamond nickel, titanium anodize gray, black and color, aluminum anodize and more.


PUBLISHED: 11/30/2016

Asterion Introduces Techniplate E-NIC 1200 High-Speed, High-Phosphorous Electroless Nickel

Provides exceptional corrosion and wear resistance as the process imparts a semi-bright deposit that is RoHS compliant and meets the stringent requirements of the ELV and WEE directives.


PUBLISHED: 11/1/2016

Electroless Nickel Technology Offers High Tolerance to Zinc Contamination

Atotech’s Nichem MP 1188 supports the mid-phosphorous EN process.


PUBLISHED: 9/14/2016

Tri-Mer Offers Tanks Over 100 Feet

The company specializes in 100-percent copolymer and homopolymer polypropylene that are rugged, long-life materials.


PUBLISHED: 8/22/2016

Crista Chemical Co. Develops Titanium Plating Process

Company says process can electroplate PEEK, ABS, PCABS, ULTEM, carbon fiber composites and carbon foam with electrolytic copper, turbo Ni/NanoNi-Co-P/alloys, electroless nickel-high phosphorus and titanium alloys.


PUBLISHED: 8/8/2016

Blue Dichtol from Stronghold Coating Systems

Blue Dichtol capillary sealer impregnates micro-pores and hairline cracks without vacuum or pressure, forming a protective barrier to gases and liquids.


PUBLISHED: 8/1/2016

MacDermid Enthone Masco 400 DM Removes Zinc Phosphate Layers

Heavy duty, low-foaming liquid alkaline cleaner also works on oils, grease, soaps and solid lubricants.


PUBLISHED: 6/20/2016

Technibrite HT 1000 Bright Tin Acid Process for Rack and Barrel Plating

Bright acid tin process suitable for rack and barrel electroplating applications iImproves appearance and performance of parts with complex geometries.


PUBLISHED: 5/24/2016

Lincoln Industries Insulation System Maintains Heat

This product’s thermosetting textile cover and insulation layers enable the technology to conform to complex part geometries.


RSS RSS  |  Atom Atom