Stripping Solvent Offers Eco-friendly Coating Removal
Dissolves powder coatings and some liquid paints at room temperature.
Solvent KIeeene’s D-Zolve 319 is a powder coating remover that dissolves powder coating and some liquid paints using an environmentally friendly chemistry. The solvent works at room temperature to penetrate and dissolve layers of both powder coat and some liquid paints, including blind holes and narrow openings. According to the company, the solvent eliminates burn-off ash and the need for high temperature. The product has no chlorinated or ozone depleting components; is nonflammable and noncarcinogenic; and has no peroxide or reproductive effect.
RELATED CONTENT
-
Coating Thickness Measurement: The Fundamentals
A review of available test methods, common applications and innovative instrumentation...
-
Improving Transfer Efficiencies in Coating Operations
There are many methods for addressing electrostatic grounding in metal painting processes, and Tim Ulshafer from Mueller Electric says the best method for your process is a simple and worthwhile exercise.
-
Phosphate Conversion Coatings
Types of phosphate conversion coatings, how to apply them, and their specific functions.