AQUEOUS CLEANING

Parts Cleaning

Parts Cleaning Clinic: Phosphate Coating Problems

Q. We electrocoat sheet metal, iron castings (machined and non-machined) and aluminum castings (machined and non-machined surfaces) and are having problems with poor phosphating on aluminum substrates. We maintain the free acid at 0.7-1.1 points and total acid at 20-24 points, and the total fluoride at 1,500 ppm. Bath temperature is 40°C to 45°C. Any suggestions?

Parts Cleaning

Parts Cleaning Clinic: Pretreatment Equipment Suppliers

Q. I am researching manufacturers of aqueous part washers and phosphate pretreatment systems for powder coating, looking for companies that build conveyor systems, washers and treatment systems; not parts washers. The parts to be cleaned are various sizes of steel, stainless and aluminum fabrications from stampings, cut to length steel tubing, and sheet metal fabrications up to 6 feet long and 3 feet wide. What are my options?

Liquid Coating

The Making of a World Class Manufacturer ... A Long-Term View

Firms empowering employees with higher skill levels will be light-years ahead.
#management #workforce development #masking

Parts Cleaning

Parts Cleaning: Does the Cleaning Agent Work?

Cleaning is a process. For this discussion, let’s focus on the cleaning agent itself. Choosing the right cleaning agent (aqueous or solvent) involves a number of factors.

Parts Cleaning

Parts Cleaning: Aqueous System Handles Tighter Cleaning Specs for Intricate Plans

Where 10 years ago, particle sizes of 1,000 microns captured in a millipore patch test might have been acceptable, today heavy equipment OEMs commonly demand maximum particle sizes of 600 microns or less.

Parts Cleaning

Parts Cleaning: Understanding the Process of Vacuum Cycling Nucleation

VCN process is accomplished by reducing the total pressure in a controlled-environment chamber that contains the components to be cleaned submerged in a solvent or an aqueous solution.
#basics #vacuum-vapor

Parts Cleaning

Parts Cleaning Clinic: Cleaning Oxygen-Free Copper

Q. Could you share with me how to lower or eliminate this defect and how to utilize automatic cleaning?

Parts Cleaning

Astro Pak Acquires Chemko Technical Services

The newly acquired AS9100 Certified Class 10,000 square foot cleanroom facility in Florida equips the company to better serve the precision cleaning, testing and passivation requirements.

Parts Cleaning

Successful Cleaning Process Requires Team Effort

Customer and supplier mount intensive effort to bring a new, successful cleaning process online.

Parts Cleaning

Cleaning Q&A: Rust on Untreated Zinc Phosphate Surfaces

The internal phosphated surface of our parts rust if no rust preventive oil is applied within two or three days.