Liquid Coating

Adhesion to Plastics

Question: Recently, I have experienced some sporadic paint adhesion failures.

Read More

An Easy Transition to Electrostatic Bells With Employee Buy-In

Changing the way you do things can be difficult. But, Grote Industries embraces change by encouraging its employees to continually generate ideas to improve its manufacturing process. This philosophy made the switch to new electrostatic bells on the painting line a rather easy one...

Read More

Finish for Stainless Steel

Question: We are looking for a navy blue finish for a 304 stainless steel cylinder that is used as a knob on one of our products.

Read More

Spraying Metallic Paints

Question: I have experienced some difficulty in color matching between methods of spray application, primarily with metallic colors.

Read More

Electrical Insulation

Question: I work with a consulting firm and I am doing research on finishes.

Read More

Spraying Inside Tubes

Question: I hope my question is appropriate.

Read More

Waterwash Spray Booth Chemicals

Question: I have two 1,400-gallon waterwash spray booths where I spray alkyd enamel bakes, polyurethanes, epoxies and waterborne paints.

Read More

High-Tech "Weaponry" for Painters

There are many things a finisher can do to reduce its coating costs and improve part quality. But, did you ever think that laser-guided spray guns would be one of them?

Read More

Painting Brass

Question: I have a design that requires the use of brass (No. 360 copper alloy). This design requires that some portions be painted (epoxy primed and polyurethane topcoated). I have no experience painting brass and/or know if this alloy is even “paintable.” Could you provide some insight into this matter and recommend how to best prepare the surface for painting?

Read More

Black Finish for Aluminum

Question: The original question from G.B. was, “I have instrument display bezels machined from 6061 aluminum plate.

Read More
Industrial Finishing Products
Free info on GFS Industrial Paint Storage units
ENGINEERED PAINT BOOTHS & FINISHING SOLUTIONS
ECOAT 2026
EPi - Black Oxide Solutions
Koch Finishing Services
Mocap Masking Caps Plugs Tapes
The Finishing Industry’s Education and Networking Resource
ENGINEERED PAINT BOOTHS & FINISHING SOLUTIONS