Optiplan automotive sandwich panels optimized via AOC rPET resin series
Incorporation of AOC’s Synolite rPET resins into FRP cover sheets enables the development of more eco-friendly truck construction.
Edited by Grace Nehls
AOC rPET resin formulations made from post-consumer waste. Source | AOC
Opitplan GmbH (Oelsnitz, Germany) and AOC (Schaffhausen, Germany) have collaborated to develop Optiplan’s ultralight, high-strength, sustainable Polydet recycled PET (rPET) cover sheets for automotive applications, incorporating AOC’s formulations derived from post-consumer rPET waste.
Optiplan develops and manufacturers a broad variety of fiber-reinforced plastic (FRP) materials made via a continuous and discontinuous manufacturing process. The materials, typically glass fiber and a resin formulation in line customer specifications for the end-use application, are used for the production of sandwich panels incorporating a structural foam core. The resulting sandwich panels are broadly used for the manufacture of refrigerated trucks, motorhomes/caravans and various construction applications.
Recent work with a global truck manufacturer realized the development of a novel range of composite cover sheets under the company’s Polydet brand. The range, offering increased strength and stiffness, in addition to more increased sustainability, incorporates AOC’s Synolite 8421-N-1 formulation.
“Replacing continuous filament mat by fabrics has helped us to increase mechanical performance, while allowing the material to be thinner and lighter,” explains Felix Bönsch, managing director of Optiplan. “At the same time, the Polydet rPET product line is more sustainable, as they are made from AOC’s rPET products, which contain PET from post-consumer waste.”
“The AOC Synolite rPET resin series are made in our operations in Ústí nad Labem in the Czech Republic. In this plant we can convert a waste product into a valuable raw material, and ultimately, into a quality formulation,” says Fons Harbers, VP marketing and sales of AOC EMEA. “The manufacturing of formulations from post-consumer waste is more cumbersome in comparison with normal formulations, as it involves additional process steps. Yet, AOC does believe that using rPET as raw material will reduce the amount of plastic waste, and is the right thing to do for the environment.”
In order for customers to better recognize products with reduced environmental impact, AOC has introduced the Next Eco-label. Besides formulations with renewable content like rPET, the Next Eco-label also covers styrene-free, low styrene and bio-based series.
With positive results in hand, Optiplan’s customer asked it for an entire range of new lightweight truck designs. Benefits of the new trucks include reduced fuel consumption and extended action radius, while maintaining the advantage of low maintenance associated with the use of composites. “In addition, the increased payload and action radius, as well as the possibility to drive a greener car contribute to the positive driving experience,“ adds Timo Hoffmann, director of sales at Optiplan.
Beyond using Polydet r-PET for lightweight truck construction, Opitplan is confident its new product will find its way in motorhomes, caravans and last-mile delivery vehicles. Additionally, the eco-friendly features of these composite sheets position them for increased use in building and construction applications, with the most obvious end markets being modular housing, wet and cold storage rooms, building façades and surface cladding.
RELATED CONTENT
-
How Ford Is Honoring the F-Series with Color
Ford celebrates 75 years of F-Series trucks with five color options.
-
Cr(III) Conversion Layers on Zinc and Zinc Alloys: Evolution and Perspectives
Trivalent chromium conversion layers have successfully replaced hexavalent conversion chromium on zinc and zinc alloys for many applications, especially in the automotive industry since the entry in force of the ELV directive.
-
Dürr Partnership Expands Market Access for EV Batteries
The Dürr Group and Osaka-based firm Techno Smart have partnered to increase EV battery production efficiency. The Dürr Group is also expanding its small-factor battery production tech business and contributing to EV production across multiple departments.