Corrosion Protection in Harsh Oil, Gas Environments
General Magnaplate’s Nedox 10K3 achieves Rockwell hardness between approximately 48 and 55 — ideal for high-corrosion environments that also cause wear and abrasion.
General Magnaplate’s Nedox 10K3 surface protection coating delivers superior corrosion protection in harsh oil and gas environments where saltwater, sour gasses and corrosive mud are present. As part of the Nedox family of coatings, 10K3 boosts the performance of common metal alloy surfaces, helping them last longer and perform better.
Nedox 10K3 achieves Rockwell hardness between approximately 48 and 55 — ideal for high-corrosion environments that also cause wear and abrasion. In salt spray tests, Nedox 10K3 showed little or no corrosion after 2,000 hours of exposure. It was also tested to and passed the 96 hour requirements of NACE
TM0284. Additional features include release properties up to 850 °F, good mating with other parts with both similar and dissimilar base materials, prevention of wear and galling and low coefficient of friction.
With Nedox 10K3, tool designers can downsize casings and make components smaller for more efficient drilling and extraction. Applications include drill string components, as well as gate, cylinder and airlock valves, housings, impellers, rotors and mud pump components.
RELATED CONTENT
-
High-Performance Primers Fight Corrosion
Interpon Redox high-performance primers from AkzoNobel offer high levels of corrosion protection.
-
CHEMEON eTCP Powder Qualifies for MIL-DTL-81706B / MIL-DTL 5541F
The DoD-qualified products list (QPL/QPD) now includes eTCP Powder for corrosion protection and improved adhesion.
-
Sol-Gel Metal Pretreatment Offers Corrosion Protection, Adhesion
The pretreatment solution is designed specifically for the aerospace industry.