Electrodeposition of Ni-Fe-Mo-W Alloys - Part 2
This paper was submitted to NASF and the AESF Foundation Research Board in July 2013 as a 2nd-quarter report of AESF Research Project #R-117.
#nasf #research
Considerations Regarding the Proper Loading of Vibratory Finishing Bowls for Optimal Quality, Performance and Throughput Efficiency
Available since the late 1950s, traditional vibratory bowl processing has advanced in recent years from being a generic deburring tool to being able to achieve high-quality, isotropic superfinishes on critical, dimensionally-challenged workpieces. This paper is a peer-reviewed and edited version of a presentation delivered at NASF SUR/FIN 2013 in Rosemont, Ill., on June 11, 2013.
#nasf #surfin #research
Electrodeposition of Ni-Fe-Mo-W Alloys - Part 1
This paper was submitted to NASF and the AESF Foundation Research Board in April 2013 as a 1st-quarter report of AESF Research Project #R-117.
#research #nasf
Corrosion Resistance of High-Phosphorus Electroless Nickel with a Lower Coefficient of Friction, Nanoparticle Codeposition Electroless Nickel Layer
This paper is a peer-reviewed and edited version of a presentation delivered at NASF SUR/FIN 2013 in Rosemont, Ill., on June 11, 2013.
#research #nasf #surfin
Are Ionic Liquids the Future of the Surface Treatment?
This paper is focused on the application of ionic liquids related to surface modification and metal deposition.
#research
Cyanide-Free Electroplating of Cu-Sn Alloys
This paper is a peer-reviewed and edited version of a presentation delivered at NASF SUR/FIN 2012 in Las Vegas, Nev., on June 13, 2012.
#nasf #surfin #research
White Bronze, Copper-Tin-Zinc Tri-metal: Expanding Applications and New Developments in a Changing Landscape
This paper deals with the renewed interest in applications for white bronze tri-metal (Cu-Sn-Zn alloy).
#research
Method for Comparison of Leveling in Decorative Acid Copper Plating
Presented here is a test mechanism used to compare and contrast systems for leveling in acid copper plating as well as additives within a system.
#research
Hexavalent Chromium - What Else?
Dr. Patrick Benaben won the 2011 NASF Scientific Achievement Award. Here is an edited version of his presentation at NASF SUR/FIN 2012, along with commentary provided by Dr. James H. Lindsay, Technical Editor for the NASF.
#research #nasf #surfin
Experimental Study on the Formation of Electroless Nickel-Boron Coatings from a Borohydride-Reduced Bath on Mild Steel
This paper is a peer-reviewed and edited version of a presentation delivered at NASF SUR/FIN 2012 in Las Vegas, Nev., on June 13, 2012.
#research #nasf #surfin