RESEARCH

Electroplating

Toward Automatic Control of Nickel Plating Processes

Technological advances in electronics manufacturing and the design of automobiles have brought about a trend toward very narrow specifications and increasingly stringent requirements on the quality of electrodeposited layers of nickel.
#research #surfin #electronics

Electroplating

Self-Induced Repair of Printed Circuit Boards

This is a re-publication of the 1992 AESF Gold Medal Award paper for best paper published in Plating & Surface Finishing in 1991.  It introduces a then-new technique for repairing near-opens (constrictions) in the wiring on printed circuit boards has been developed.
#research #electronics

Electroplating

Surface Finishing in the 2000s - As Predicted in 1992

In the December 1992 issue of Plating and Surface Finishing, a series of articles was published, predicting the future of the global surface finishing industry in the 21st century, then due to arrive in less than a decade.
#research #surfin

Anodizing

Impact of Intermetallic Species on Cast Aluminum Alloys for Anodizing Applications

Alloys with higher silicon concentrations can inhibit the growth of anodic oxide films under galvanostatic and potentiostatic conditions.
#research

Electroplating

The Relationship Between Vickers Hardness and Universal Hardness

The Vickers indenter hardness test, based on indenter displacement under test load (universal hardness), is being used for an increasing number of applications.  The new method is also subject to much discussion among the experts.  An important question is the relationship or the degree of correlation between the new universal hardness test and the classic Vickers hardness test.
#research

Electroplating

Evaluation of a Simple Thin-Film Ductility Tester and Review of the Ductility of Nickel Sulfamate Deposits

Originally published in 1992, this paper addressed a critical issue in the science of electroforming, that of the measurement and control of deposit ductility.
#research

Electroplating

Electrocodeposition of MCrAlY Coatings for Advanced Gas Turbine Applications - 5th Quarterly Research Report

The objective of the work is to study and optimize the MCrAlY electrocodeposition process to improve the coating oxidation/corrosion performance. In this quarter, work focused on preparation and characterization of CrAlY-based alloy powders for the planned research activities in Task 2: The Effect of CrAlY Particle size on CrAlY Particle Incorporation.
#research

Electroplating

Advancements in Brush Plated Metal Matrix Composites

Finding safer, eco-friendly alternatives to hard chromium plating has been a main driver of brush electroplating research for the last decade.
#research #surfin

Electroplating

The Mechanism of Nickel Corrosion in ENEPIG Deposits and How to Mitigate It

The incident of nickel corrosion in ENEPIG multilayers (electroless nickel, electroless palladium and immersion gold) was brought to light after it was observed during the analysis of gold wire bond lifts.
#research #basics #surfin

Electroplating

Nanoporous Anodic Oxides: Fabrication, Applications, Sensing and Biosensing

Numerous metals are subjected to anodic oxidation. As a result, one can obtain amorphous barrier-type oxides, crystalline barrier-type oxides or amorphous nanoporous oxides. This paper provides details of sensing techniques and recent advances in the development of NAA-based sensing and biosensing technologies.
#surfin #research