VIDEO: Mercedes-Benz Picks Ecopaint RoDip for New SC Plant

Rotating vehicles up to 26 feet long through an immersion bath is something that has never happened before, says Dürr Group, one of the world's leading mechanical and plant engineering firms with automation expertise.
#automotive

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon
c

 

 

Rotating vehicles up to 26 feet long through an immersion bath is something that has never happened before, says Dürr Group, one of the world's leading mechanical and plant engineering firms with automation expertise. 

But the Ecopaint RoDip rotational dip process is now being used for the first time for vehicles of this size. Dürr will be installing this technology in the new Mercedes-Benz Vans factory in North Charleston, South Carolina. It will form part of a complete paint shop being built by Dürr on behalf of Mercedes-Benz Vans. Completion is expected by 2020.

Even very large car bodies — such as those of transporters and vans — can rotate around their own axis with a rotational movement of 360°. When planning the plant in North Charleston, Dürr conducted extensive tests in its technical center. This included testing ways of using the RoDip rotational dip process for painting car bodies larger than had ever been immersed before. The result? RoDip guarantees high-quality corrosion protection as a basis for further surface coating, even for large vehicles.

The system will transport the closed car bodies of the next generation of the Mercedes-Benz Sprinter through pretreatment and cathodic electrocoating. Each of the freely programmable transport units has a separate drive for rotation in addition to the conveying drive. 

The individually programmable transport units enable optimized dip curves for the respective car body. The end result is better coating quality and increased energy efficiency. The rotational process means that smaller bath volumes are possible; these require less volume of chemicals and fresh water while reducing the energy consumption and volume of wastewater.

Mercedes-Benz Vans announced its plans to extend its existing assembly location for vans and build a new factory for the production of the Mercedes-Benz Sprinter in 2015. Production is due to start before the end of the decade. Until then, Sprinters for the U.S. market will be manufactured in Germany. Due to high import duties, however, they will be partially disassembled in a complex process and reassembled in the plant in North Charleston.

According to Daimler, this additional step puts Mercedes-Benz Vans at a clear competitive disadvantage in the US market. The new factory and vehicles “made in USA” will enable the division to service the growing demand from North American customers much more economically in the future, and significantly reduce the delivery times in the market. The division is investing approximately $500 million in the construction of the factory. Mercedes-Benz Vans is the only manufacturer in the large transporter segment that is still manufacturing in Germany.

Get more information HERE.

 

 

Related Topics

RELATED CONTENT

  • Cyanide-Free Electroplating of Cu-Sn Alloys

    This paper is a peer-reviewed and edited version of a presentation delivered at NASF SUR/FIN 2012 in Las Vegas, Nev., on June 13, 2012.

  • Building an E-coat Line from the Ground Up

    How one company is prospering by providing flexible e-coat capability to Nissan and other customers.

  • Measuring the Surface Area of Fasteners

    How do you measure the surface area of a threaded fastener? How much coating would you put on it? How thick of a coating? What about non-threaded fasteners? The U.S. Department of Agriculture’s Forest Service, of all people, may have come up with the solution for those pondering how to coat sometimes-difficult small pieces using computer imaging and software to compute the area.