Nasmyth TMF Achieves NADCAP Accreditation for Non-destructive Testing
Metal finishing, painting and non-destructive testing specialist Nasmyth TMF has achieved NADCAP accreditation for non-destructive testing services for the aerospace and defense industries.
#military #aerospace #measurement-testing
Edited by Scott Francis
Nasmyth TMF (Valencia, Calif.), a specialist in metal finishing, painting, and non-destructive testing for the aerospace and defense industries, has achieved NADCAP accreditation for its non-destructive testing (NDT) services.
Francisco Palop, General Manager of Nasmyth TMF, notes: “With our ongoing full Nadcap accreditation we are well placed to continue serving the aerospace and defence supply chains across the USA and Canada.”
RELATED CONTENT
-
Coating the Webb
From its signature primary mirror to thermal control for its instruments, the James Webb Space Telescope is enabled by gold coatings.
-
Stripping Metallic Coatings
The stripping of electrodeposited and flame-sprayed coatings is a necessary part of surface finishing. Stripping may be required to allow for the re-plating of a part rejected due to defective finishing or as part of rework processes such as those commonly conducted by airline/aerospace facilities. This paper discusses stripping methods and operational considerations in their use.
-
Anodizing for Bonding Applications in Aerospace
Anodizing for pre-prep bonding bridges the gap between metallic and composite worlds, as it provides a superior surface in many applications on aluminum components for bonding to these composites.