Anodizing Clinic: Measuring Color of Coatings with a Colorimeter

Q. Recently, a company asked us to match its samples so we could do work for them. According to our method, we matched the samples, but they were rejected when they were sent to the company. We were told the samples were out of tolerance. We discovered the company used a different brand colorimeter with a different color scale to measure the color. Is there a set standard in the anodizing industry for measuring and matching colors?

Anodizing

Anodizing Clinic: Anodic Coating Blistering on 7075 Alloy

Q. We have recently run into a surface condition when hard anodizing 7075 machined forgings. It seems to be present primarily on the end of the part, even down into the hole. Both of these areas are machined. The condition does not appear to be evident on other surfaces. I have not seen this condition before, but it appears to me to be rather unique and something recognizable.

Anodizing

Aerospace Finishing’s Race to the Moon

In our 80th year, a look back at how finishing helped NASA-led space projects.
#aerospace

Parts Cleaning

80 Years Helping Finishers

Our readers share how Products Finishing has helped their careers as the magazine celebrates its 80th year covering the finishing industry.
#curing #pollution control

Anodizing

Anodizing Helps Yo-Yos Make a Colorful Comeback

One Drop Yo-Yos in Eugene, Oregon, is a leading high-end yo-yo manufacturer. It gets some of the 8,000 products it makes finished at Gruntbull Anodizing in Gettysburg, Ohio, whose splash anodizing process combines as many as six colors on the same part. The result is a piece of art.

Electroplating

Coating to Help Europe's Telecom Satellites Keep Their Cool

A surface coating originally developed for medical implants is set to safeguard the next generation of European telecom satellites.
#medical #masking #pollution control

Anodizing

Jack Humble on the Value of Aluminum Anodizers Council

As term on the Board of Directors draws to a close, Humble expresses appreciation to everyone at the AAC on a rewarding and fulfilling experience.

Powder Coating

Greenkote Adds Major Anti-Corrosion Coating Capacity in Ohio

The company says that the added equipment will multiply current capacity by nearly two and a half times, enabling the Brook Park facility to process more than 150 tons of parts per month.
#masking

Electroplating

ASETSDefense Workshop 2016: Sustainable Surface Engineering for Aerospace and Defense

Workshop on Sustainable Surface Engineering for Aerospace and Defense will be held at Shades of Green, the Armed Forces Recreation Center at the Walt Disney World Resort in Orlando from December 6-8.
#military #aerospace #sustainability

Anodizing

Anodizing: Corrosion on Hardcoat Anodized 7000 Series Forging

Q. I sent you photos of two parts that are alloy 7050 forgings. On these parts there are spots that appeared as a result of Type III (hardcoat) anodizing that were not present before anodizing. They look like corrosion of some sort, but the corrosion looks a little different on each part. What causes these spots to appear and what measures can be taken to prevent or eliminate them after they occur?